Dear Sir
Please support us for below concern:
i carried out PQR with GTAW & SMAW (No Impact, GTAW deposit weld is 5 mm & SMAW deposit weld is 42.64 mm), the test coupon is 23.82mm so the qualified thickness range will be 5 to 47.64 mm.
Regards
--