IMPACT TEST REQUIREMENT

100 views
Skip to first unread message

balaji srinivasan

unread,
Jun 17, 2016, 3:55:27 AM6/17/16
to material...@googlegroups.com
Dear All,


As per ASME SEC-IX   change in material Group is Supplementry  essential variable (403.5)

based on above i need your experience  If iam qualified PQR p1 group-1 to p1 group-2 tow different group welded it self so the  qualfied range will be p1 group1 and p1 group 2.

or only this PQR is qualified group 1 to group-2 qualified.

also please advice i need to qualify group 1 separate and group 2 separate PQR.


nithind...@gmail.com

unread,
Jun 17, 2016, 6:52:49 AM6/17/16
to material...@googlegroups.com
P1 G1 to P1 G2 qualifies P1 G1 to P1 G2, P1 G2 to P1 G2 and P1 G1 to P1 G1. Hope your query is addressed.

Sent from my iPhone
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK1csg3Drkobg2%3DG9Lyy0CMd3WbM%2BOq_9e2GkJLoC-QxBUhP0A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Mohammed Rafiuddin

unread,
Jun 18, 2016, 6:59:16 AM6/18/16
to material...@googlegroups.com
PQR on P1Gr1 to P1Gr2 qualifies welding P1Gr1 to P1Gr2 only and NOT welding to themselves i.e ( P1Gr.1 To P1Gr1 Or P1Gr2 to P1Gr2)

Refer ASME interpretation IX-92-70 on the same subject.I could not find downlodable copy.Try to search on internet.

Thanks
Mohammed


Raghuram Bathula

unread,
Jun 18, 2016, 7:12:16 AM6/18/16
to Materials-Welding
Mohammed: interpretation IX-92-70 does not address this situation
Balaji : You can use this PQR for welding P1 G1 to P1 G2, P1 G2 to P1 G2 and P1 G1 to P1 G1

George Dilintas

unread,
Jun 21, 2016, 10:26:22 PM6/21/16
to Meghanadh K
No, if you read carefully the last sentence of 5th paragaphe of QW-403.5 the combination in the same test coupon qualifies the group numbers to themselves.
However if the application Code Section (VIII-1, VIII-2) does not require HAZ impact testing you dont have to worry about this variable


For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis