A335 P11 can be used instead of P22

183 views
Skip to first unread message

Chiranjeevi A

unread,
Jun 27, 2019, 6:17:31 AM6/27/19
to material...@googlegroups.com
Dear all,

We have a situation that we need to weld cap (material P11) to weldolet with P22 material. Size 2" NPS. Line temp is 560C and pressure 48bar. The rating of the main header is 1500# P22 mtl. Can we weld to the following conditions P11 mtl cap to weldolet P22 mtl.

Carlos Arturo Oliveros Diaz

unread,
Jun 27, 2019, 11:29:03 PM6/27/19
to material...@googlegroups.com
Dears, 
Your requirement Install the same material that is in the material of the invoice, the approved Engineering Department must be changed before being approved, it should not be changed


Carlos Arturo Oliveros Diaz  +573023482020

1472502898497_Inspector.jpg            ws+584245923932



De: material...@googlegroups.com <material...@googlegroups.com> en nombre de Chiranjeevi A <chiranjee...@gmail.com>
Enviado: jueves, 27 de junio de 2019 5:03 a. m.
Para: material...@googlegroups.com
Asunto: [MW:29753] A335 P11 can be used instead of P22
 
Dear all,

We have a situation that we need to weld cap (material P11) to weldolet with P22 material. Size 2" NPS. Line temp is 560C and pressure 48bar. The rating of the main header is 1500# P22 mtl. Can we weld to the following conditions P11 mtl cap to weldolet P22 mtl.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0wXZEi-VoDnnHJRypawcopE%3DSoK2E0va9iJd3C1gTPJAQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

pradip kumar Sil

unread,
Jul 1, 2019, 3:54:29 AM7/1/19
to materials-welding
Before change the material , consult with your design team

munee...@gmail.com

unread,
Jul 1, 2019, 3:54:33 AM7/1/19
to materials-welding
Hi, 

If header pipe is P5A why it is connected with P4 CAP (Tie-in point)? in which P5A weldolet to be fused with P4 CAP? is that your query? 

Is this pre approved design or shortage of material? so you just inserting one what you have?

write a TQ to ''the company'' take approval with disimilar WPS.

I hope there shall not be an issue if you are proposing with your adjustment in case, but designers approval is final.

Yours
MOHAMED MUNEEB MAHABOOB
+91-786-700-444-6      TRZ - INDIA
''do that quality job - which doesn't promise your tomorrow''

--

Kannayeram Gnanapandithan

unread,
Jul 1, 2019, 4:13:03 AM7/1/19
to materials-welding
P22 has got more Creep Strength at High temp compare to P11

George Dilintas

unread,
Jul 9, 2019, 11:18:11 PM7/9/19
to material...@googlegroups.com
No withou design calculations 

Στις Πέμ, 27 Ιουν 2019, 13:17 ο χρήστης Chiranjeevi A <chiranjee...@gmail.com> έγραψε:
Dear all,

We have a situation that we need to weld cap (material P11) to weldolet with P22 material. Size 2" NPS. Line temp is 560C and pressure 48bar. The rating of the main header is 1500# P22 mtl. Can we weld to the following conditions P11 mtl cap to weldolet P22 mtl.

--