ASME SA105 Quenched and Tempered

47 views
Skip to first unread message

Umar Rashid Makrani

unread,
Nov 27, 2016, 7:50:43 AM11/27/16
to Materials & Welding
Dear Mentors,
As per Product specification SA105 marking "QT" is required if the forging is Quenched and Tempered.
in one of the MTC the material mentions as Quenched and Tempered but the marking QT is NOT found.

Please advice 

Regards

George Dilintas

unread,
Nov 27, 2016, 9:46:04 PM11/27/16
to Meghanadh K
for pipes and fitting marking prevails. NCR should be issued and further investigation should be undertaken

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d66a3b8a-9e1f-4238-b3ca-a7151f40ea8d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

anthony chundal

unread,
Nov 27, 2016, 9:46:31 PM11/27/16
to material...@googlegroups.com
Dear Umar,

You can ask the manufacturer to provide a letter of conformity stating that the stamping was missed out and they authorize you to do the same. If it is an coded vessel then please take the concurrence of the AI by raising an NCR. or  else you can inform your client about the same. but most important is if there is impact testing then you have to follow below,

Inline image 1

Thanks & Regards,
Anthony.


--