Clad As per Sec IX

38 views
Skip to first unread message

K K

unread,
May 20, 2019, 8:09:26 AM5/20/19
to Materials & Welding



Dear All,


We have three sort of clad,

 

CS + 825 clad pipe  (filler metal ERNiCrMo-3)

CS + 625 weld overlay pipe (filler metal ERNiCrMo-3)

CS + 316 clad pipe (filler metal ER 309 Mo)

 

As per ASME IX,  if welders need to be qualified in clad pipe or they can be qualified in CS regular pipes (QW-383)


Please give me your feedback.


Thanks and Regards

K K

George Dilintas

unread,
May 21, 2019, 5:34:12 AM5/21/19
to material...@googlegroups.com
QW-380 and QW-383 are crystal clear. The best way to go ahead is to implement  QW- 383.1(b)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7b831e8e-2e13-466d-abee-53248af13818%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Prakash Hegde

unread,
May 21, 2019, 5:34:17 AM5/21/19
to material...@googlegroups.com



On Mon, 20 May 2019 at 17:39, K K

Hi!

 For clad restoration you rrequire to qualfy for Overlay in the particular position as per ASME sex IX satisfying all overlay qualification requirement

For base metal welding you should  qualfy welder satisfying Sec IX Groove weld requirement

Regards

Hegde

--