| From: SATISH SHAH Sent: Σάββατο, 21 Μαΐου 2016 - 05:51 To: Materials & Welding Reply To: material...@googlegroups.com Subject: [MW:24816] Ferrite % 4-8 of E309LMo |
How much did you get on PQR?.
ferrite depend on many other factor other than just filler wire.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---