I have a doubt, how often we can repair weld for AISI 4130 material.
How many repair welds can be done on a AISI 4130 material.

Kindly advise.

Regards,
M. Sivachidambaram
0559212392

George Dilintas

unread,
Feb 17, 2017, 9:44:08 PM2/17/17
to Meghanadh K
It is a low alloy steel, so in case of a second repair is better to prepare a moque-up

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMUQbpUDNy61fhf7QkDqeW1DzChENb1x2azOTFJbDv36Sw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

chandrakant mohikar

unread,
Feb 17, 2017, 9:45:27 PM2/17/17
to material...@googlegroups.com
Dear Mr. M. Siva

Sometimes the philosophy of constructability and or operability is
complete remote operated. The numbers of repair can be as per owner’s
requirements and considerations. E.g. if equipment / component of AISI
4130 steel and it is installed in remote place / desert where the
facilities are unmanned / unattended. It, the joint, should not be
repaired at all for safety reasons mentioned above (unmanned).
Multiple repair of AISI 4130 may result in consequences that cannot be
controlled and very difficult to control release of hazardous fluid /
chemical in equipment.

Separate lengths are joined by connectors, normally made of AISI 4130
steel. In non-corrosive environments these are protected by nickel
plating on the surface. For corrosive environments it is preferable to
weld-overlay the entire surface with Alloy 625.

Its’ high-strength properties at high temperatures, AISI 4130, a
chromium -molybdenum alloy steel, is used in automotive like
experimental airplanes, racing car frames, roll cages, go-carts,
Bicycles and motorcycle frames. Other uses include petrochemical and
steam-tubing applications. Typically, this alloy contains about 0.30
percent carbon.

it is better to fabricate 1st time right and it must be flawless, perfect.

Chandrakant Mohikar
ex. PDO (Company site representative / Project QA)
8446079514
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-weld...@googlegroups.com.
> To post to this group, send email to material...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages