Dia range.for WPS as per API 1104

2,191 views
Skip to first unread message

joydev dalai

unread,
Apr 21, 2018, 2:27:35 AM4/21/18
to materials-welding
Dear Expert,

Please suggest Dia range.for WPS as per API 1104.

--



Best Regards,

Joydev Dalai
Dy. Manager - QA/QC
Kalpataru Power Transmission ltd.

CEIL Mumbai

unread,
Apr 21, 2018, 6:17:31 AM4/21/18
to material...@googlegroups.com
For PQR/WPS no dia range

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

ramen samanta

unread,
Apr 21, 2018, 10:47:49 PM4/21/18
to material...@googlegroups.com
Dear Joydev

Pl. ref. API- 1104- clause 6.2.2 (d)- dia. groups

Thanks,

R.K.Samanta



CEIL Mumbai

unread,
Apr 22, 2018, 12:12:22 AM4/22/18
to material...@googlegroups.com
6.2.2(d)is for war not for wps

Kannayeram Gnanapandithan

unread,
Apr 22, 2018, 1:09:15 AM4/22/18
to materials-welding
Non essential. There is no limit on pipe dia. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sun, Apr 22, 2018 at 9:40 AM, CEIL Mumbai <bppl...@gmail.com> wrote:
6.2.2(d)is for war not for wps

On Sun 22 Apr, 2018 8:17 am 'ramen samanta' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear Joydev

Pl. ref. API- 1104- clause 6.2.2 (d)- dia. groups

Thanks,

R.K.Samanta



On Saturday, 21 April, 2018, 11:57:31 AM IST, joydev dalai <joykol...@gmail.com> wrote:


Dear Expert,

Please suggest Dia range.for WPS as per API 1104.

--



Best Regards,

Joydev Dalai
Dy. Manager - QA/QC
Kalpataru Power Transmission ltd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Ramesh

unread,
Apr 23, 2018, 2:47:01 AM4/23/18
to material...@googlegroups.com

Hi

API 1104 covers welding procedures qualifications as below,

Case

1.    Clause 5 Welds Containing Filler-metal Additives

2.    Clause 12 Mechanized Welding with Filler Metal Additions

3.    Clause 13 Automatic Welding Without Filler metal Additions

 

 

Diameter range is not essential for case 1 WPS/PQR, i.e. 5.3.2.3 however “the ranges of outside diameters and wall thicknesses over which the procedure is applicable shall be identified”.

 

Means unlike ASME sec 9, WPS/PQR format, additionally you may need to specify the restriction on outside diameter and thickness in order to facilitate to have control on welders use in production welding ( based on clause 6.2.2 d )


Diameter range for case 2 & 3 WPS/PQR is essential variable, refer respective clauses - 12.5.2.5 & 13.5.2

 

 

Also refer API 1104 interpretation ( specifically Page 82 /94 ) attached herewith for more details. There are many questions based on this topic only.

 

Downloaded from

http://mycommittees.api.org/standards/techinterp/transpipe/default.aspx

 

 


1104.pdf

Rajeev Shukla

unread,
Oct 22, 2020, 12:35:04 AM10/22/20
to Materials & Welding
Sir

I need to under stand the meaning of this line , and which code I should refer for Compressor received welding.

Longitudinal seam in adjacent sections shall not be in same line.

nandakumar pandit

unread,
Oct 22, 2020, 12:42:28 AM10/22/20
to material...@googlegroups.com
This means if your shell is in sections, then the longitudinal weldings in all the sections should not be in the same line.

Regards
N. S. Pandit



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c23d7c90-1f2b-4a58-ab4d-651cbde1c374n%40googlegroups.com.

Rajagopal Kannan

unread,
Oct 22, 2020, 12:51:11 AM10/22/20
to material...@googlegroups.com
Hi,
You Should not have "+" shaped joint.
Thanks and Best Regards,
K.Rajagopal

vijay konathala

unread,
Oct 22, 2020, 8:14:49 AM10/22/20
to material...@googlegroups.com
pls reffer the attachment which will help you .

which tells about various codes which follows thumb rules as specified

With regards 
vijay kr Konathala
7995602589  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c23d7c90-1f2b-4a58-ab4d-651cbde1c374n%40googlegroups.com.


--

With Regards
Vijay Kumar Konathala
minimum distance of weld joints.png

Kannayeram Gnanapandithan

unread,
Oct 22, 2020, 10:57:13 AM10/22/20
to materials-welding
Lseam  of 2 shell shall not be in line, it shall be kept at 5XThickness of shell in staggered position
All code and std are specifying the requirement, check in section 8
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Thu, Oct 22, 2020 at 10:05 AM Rajeev Shukla <gkpsh...@gmail.com> wrote:

GENE MATSKO

unread,
Oct 23, 2020, 12:03:38 AM10/23/20
to material...@googlegroups.com
You might picture in your mind how 'bricks' are laid out or 'concrete blocks'. The Horizontal seams are continuous, however; the 'verticals' are 'offset'. This
is done to prevent a 'crack' starting in one vertical joint from propagating into the next vertical joint. If all the verticals were in one continuous joint, the crack
could propagate from the 1st, into the 2nd, into the 3rd. etc. I hope this helps.

Gene Matsko


atul khatri

unread,
Oct 23, 2020, 9:57:03 AM10/23/20
to material...@googlegroups.com
Dear Mr. Rajeev,
If your query is related to Pressure vessel then refer UW-9 (d) of ASME VIII DIV 1, which states that..
 "Except when the longitudinal joints are radiographed 4 in. (100 mm) each side of each circumferential welded intersection, vessels made up of two or more
courses shall have the centers of the welded longitudinal joints of adjacent courses staggered or separated by a distance of at least five times the thickness of the thicker plate.


One advice: Please put a proper subject to your email if you want to get it noticed by a large number of group members.


Special thanks to Mr. Vijay Konathala for sharing the thumb rules of different codes / standards for quick reference. 



Regards,
Atul Khatri
Principal Engineer- Piping
Haldor Topsoe India Pvt. Ltd


Muhammed Ibrahim PK

unread,
Oct 27, 2020, 7:45:34 AM10/27/20
to material...@googlegroups.com
Hi, 

Did you noticed when constructing building the mason not keeping the brick one over another in same position. The first brick will start from corner, the second line will start by keeping the edge of brick at center of bottom one overlapping. No buildings bricks will be exactly one over another. Use this logic, to make sure the strength of the building. 

Similar way the longitudinal seam of one shell shall not be in same line as it weakens the joint. 


George Dilintas

unread,
Nov 2, 2020, 4:00:23 AM11/2/20
to material...@googlegroups.com
Welds shall not form a cross. There is a rule for staggering, 4 times the thickness of I am not wrong

Vinay Thattey

unread,
Nov 2, 2020, 10:52:00 PM11/2/20
to material...@googlegroups.com, gkpsh...@gmail.com
Dear Rajeev ;
You need to have circumferential welds to join two shell parts . A shell is rolled from a plate with seam welds . 

Kannayeram Gnanapandithan

unread,
Nov 2, 2020, 11:43:33 PM11/2/20
to materials-welding
Shell course Lseam shall not be in line, it shall be stagged like a T joint

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

Reply all
Reply to author
Forward
0 new messages