Re: [MW:29578] Welding HSLA to Aluminium

16 views
Skip to first unread message

PREM SHANKARDUTT NAUTIYAL

unread,
May 10, 2019, 10:24:30 PM5/10/19
to material...@googlegroups.com
Not possible by Arc welding..
Try other alternatives..


PREM S NAUTIYAL
CELL : 9769316004





From: Ram <rames...@gmail.com>
Sent: Fri, 10 May 2019 11:32:55 GMT+0530
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:29578] Welding HSLA to Aluminium

I need to weld High Strength Low Alloy Steel to Aluminium Alloy 5052-H32 by MIG Welding Processes. What kind of MIG filler wire I should select.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https:roups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e88411a3-e3eb-408d...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

George Dilintas

unread,
May 14, 2019, 1:21:35 AM5/14/19
to material...@googlegroups.com
If you achieve this you will get the Nobel price. You cannot weld aluminum to steel since Al anf Fe do not form solid solution. You have to use intermediate pieces of explosion bonded Al and steel

Στις Παρ, 10 Μαΐ 2019, 09:02 ο χρήστης Ram <rames...@gmail.com> έγραψε:
I need to weld High Strength Low Alloy Steel to Aluminium Alloy 5052-H32 by MIG Welding Processes. What kind of MIG filler wire I should select.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.