pre heat inconel-625

120 views
Skip to first unread message

Ali Zarasvandi

unread,
Jun 19, 2016, 12:04:55 PM6/19/16
to Materials & Welding
hi

do we need preheat of electrode when using inconel-625









C.Muni

unread,
Jun 20, 2016, 7:06:30 AM6/20/16
to material...@googlegroups.com
Its not preheating.Its baking.Its required.Follow as per manufacturer guidelines.

Regards,


 Muniyandi Chithiran MBA.,MIIF,
AWS Certified Welding Inspector,
ISO 9001,14001,17025, Lead Auditor,
NDT Level II-RT,UT,MT,PT,

Mobile: 0091 95855 40965,99947 65591

Go where you are celebrated not where you are tolerated.
Comfort is the enemy of achievement.

On Sat, Jun 18, 2016 at 6:50 PM, Ali Zarasvandi <ali.zar...@gmail.com> wrote:
hi

do we need preheat of electrode when using inconel-625









--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e9e2daff-7d56-4611-aa40-97edced03eef%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

zakir ali

unread,
Jun 20, 2016, 7:06:48 AM6/20/16
to material...@googlegroups.com

Yes...
These electrodes are basic coated.
And hygroscopic in nature...


Sent from RediffmailNG on Android
--

Rajnish Dixit

unread,
Jun 20, 2016, 10:45:46 PM6/20/16
to material...@googlegroups.com
Dear Ali,

The term 'baking or drying' is used for heaing of the electrodes before starting welding.

You have to refer Manufacturer's recommendations & ASME Section II Part C for reference.

Regards,
Rajnish

--------------------------------------------
On Sat, 6/18/16, Ali Zarasvandi <ali.zar...@gmail.com> wrote:

Subject: [MW:24973] pre heat inconel-625
To: "Materials & Welding" <material...@googlegroups.com>
Date: Saturday, June 18, 2016, 5:20 PM

George Dilintas

unread,
Jun 21, 2016, 10:26:47 PM6/21/16
to Meghanadh K
Baking or not depends on the kind of coating (in case of covered electrodes)


For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward