Weld Symbol Description

66 views
Skip to first unread message

Nazrulla Khan

unread,
Feb 18, 2015, 11:59:21 AM2/18/15
to material...@googlegroups.com
Gents,

Can any one explain the attached image weld symbol explanation.

1.      8
2.      7
3.      2
4.     45deg

Thanks & Regards
Nazrulla.JK
weld symbol definition.jpg

John Henning

unread,
Feb 18, 2015, 12:39:38 PM2/18/15
to material...@googlegroups.com

See below:

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Nazrulla Khan
Sent: Wednesday, February 18, 2015 10:58 AM
To: material...@googlegroups.com
Subject: [MW:22901] Weld Symbol Description

 

Gents,

Can any one explain the attached image weld symbol explanation.

1.      8 – depth of bevel
2.      7 – (5?) leg lengths of fillet weld
3.      2 – root opening of groove

4.     45deg – groove angle

 

Thanks & Regards

Nazrulla.JK

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPVF%2B2PUK7BF1zNpYvf_5bDKPS7F4z-iPVtem07Lj126t5CcsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Siva Chidambaram

unread,
Mar 3, 2015, 2:44:05 AM3/3/15
to material...@googlegroups.com
Hi,
 
the detail of the weld symbol is that as follows.
1. the root gap of the first bevel joint is 2mm.
2. the Bevel angle should be 45 deg.
3. the bevel groove weld depth is 8mm.
4. after groove weld, fillet weld of leg length 5mm to be welded.
 
Thanks,
 
M. Sivachidambaram
QHSE Engineer

--