Dear All,
Need your help,
I have qualified fillet weld PQR with following ,
Thickness of Pipe:- 1 mm
Thickness of Plate :- 4 mm
I have confusion about base metal qualification thickness,
Qualification thickness will be 0.7 mm to 8 mm for single layer for both Pipe & Plate
Or
For Pipe it is 0.7 to 2 mm & for plate it is 3-8 mm.
What is correct?
Thank you
Vijay Katkar