IQI selection.

55 views
Skip to first unread message

Prabir Kumar Singh

unread,
May 25, 2016, 7:04:41 AM5/25/16
to materials-welding

What is effective thickness for IQI selection in DWSI and DWDI method. Sum of double wall thickness or only single wall thickness?

PREM SHANKARDUTT NAUTIYAL

unread,
May 25, 2016, 10:54:58 PM5/25/16
to material...@googlegroups.com
IQI selection will be based on nominal single wall thickness plus estimated reinforcement only.
Refer ASME Sec V article 2.

PREM S NAUTIYAL
CELL : 9769316004
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOis+9vAHjU6WCt_zT1Lgxze...@mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >
Reply all
Reply to author
Forward
0 new messages