Dear Kumar,
If it is E7018-1 & if impact testing is there then the cert has to be 3.1 which will give you the tested values ,as 2.2 will only give you values as per code.
Thanks & Regards
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp9j4g08J_sEsjtQ15OF2%2BUyZh8k1v9ky8arTPB53bbVtA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4qKAcVHHN5Bt%3D%2Bux8q0JL_niipD%3Dwc7nj%3Dm_pu%3DgJdp4aQ%40mail.gmail.com.
Hello Anthony,
Please see my notes on the attached MTR (Product Certificate). I do not think there is any issue in reporting of the data as per ASME Sec-II, Pt-C, SFA,5.1.
Thanks.
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
To unsubscribe from this group and stop receiving emails from it, send an email
to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp_TbeE6YTkp6n1e1g-huVW9F2fOFHOXecReE72Ey%2BfKmA%40mail.gmail.com.