Dear All,

Code: ASME SEC VIII-1

Post forming Heat Treatment of Dish...

MOC: SS316L

Design Temp 85°C

Fibre Elongation: 3.6%

UHA-44 table does not show values of Fibre elongation..

Is PFHT required for this dish.

Kindly advise

Ahmed

Prasad Ghanekar

unread,
Aug 21, 2016, 9:09:55 AM8/21/16
to material...@googlegroups.com

PFHT is not mandatory as per code.
Some client specify PFHT as solution annealing if hardness after forming is more than 22 HRC

PVG

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BL7tiPwcXf8BVFYiF_b%2BCF3jdfsjhVdQGAyK-FfvAhpWOZDOQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Prakash Gotimukul

unread,
Aug 22, 2016, 3:45:30 AM8/22/16
to materials-welding
I agree

Rgds
Prakash Gotimukul
AIS, Consultant ASME/ISO/PED/IBR

Mhaskar Aly

unread,
Aug 23, 2016, 2:24:40 AM8/23/16
to material...@googlegroups.com
Dear Mr. Prasad,
What if Fibre elongation exceed 20% (for SS316L Dish), PFHT required or not; please provide Code reference.
Thanks
Aly

On Sun, Aug 21, 2016 at 4:07 PM, Prasad Ghanekar <prs...@gmail.com> wrote:

Mhaskar Aly

unread,
Aug 23, 2016, 6:11:23 AM8/23/16
to material...@googlegroups.com
Hi all,
Refer attached discussion on this topic...

Aly