RE: MATERIAL SPECIFICATION

143 views
Skip to first unread message

VIshal Suthar

unread,
Oct 1, 2019, 4:15:37 AM10/1/19
to material...@googlegroups.com
Dear Members,

Please note one of equipment client specification mentioned Tubesheet material SA 336 F 316L.

Reference to ASME Sec-II Part A SA336 is for Alloy Steel Forging which not having 316L.

Please provide your valued suggestion.

Regards,
VIshaL SUTHAR

Raghuram Bathula

unread,
Oct 1, 2019, 4:45:30 AM10/1/19
to Materials-Welding
it should have been SA965

-- 

NISARG KEDAR

unread,
Oct 3, 2019, 6:22:49 AM10/3/19
to material...@googlegroups.com
It's a typo error. Just confirm with client if need to go with SA965 F 316L or any low alloy grade from SA 336.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOZ%2B%2BqCknkahgMMvgfnX_KZs02j5MOZ_uppOzVPPyiK96uRoJA%40mail.gmail.com.

Vinay Thattey

unread,
Oct 13, 2019, 11:20:24 PM10/13/19
to material...@googlegroups.com, vishalsu...@gmail.com
Dear ;

Unable to understand exactly what are you looking for ?? U can refer Table -1 of SA336 /336 M . Austenitic steel grade F316 L is available .  SA-336 Grade F316L, ASME, SA-336/SA-336M, are Alloy Steel Forgings for Pressure and High-Temperature Parts. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmOM3BA7xx8zqD6DNMs2nqT6E-yVLj%2BGJ1Nk9A%3DybcPkg%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages