gents,

pl advise welding of 4145H, thk-25mm dia-8"

Electrode selection,Preheat,PWHT...

with SMAW, or SMAW+GTAW

Mohd.

YOGESH JOSHI

unread,
May 26, 2021, 5:22:18 AM5/26/21
to material...@googlegroups.com
DEAR Sir, 

It is D&H Secheron make CNM Spl M product suitable for this welding. 