Define welding engineer

89 views
Skip to first unread message

JERRY TUAN

unread,
Jan 15, 2016, 8:55:34 PM1/15/16
to Materials & Welding
My company need to qualify wps follow aws d1.1 :2010 . And we do run pqr by testing internal, witness test piece . Only send test piece to third party LAB to bend test and RT. But not have third party witness all process from starting. So my question is : do we do wps right with spec aws d1.1
- does spec or code require wps must have third party to witness , cause I can not find any information about it

Thanks very much all experts
Tuan QC inspector

José Juan Jiménez Alejandro

unread,
Jan 15, 2016, 11:19:35 PM1/15/16
to material...@googlegroups.com
You should use D1.1 2015 edition, this is the latest version of this code. You do not need to have a third party for inspection this witnessing tests, usually the code responsible for the manufacturer of the application of welding, the WPS, PQR and qualification of welders is your responsibility to your company, as well Czech the code says about it.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1b8824bd-f8f8-4272-9ce1-de21585a0051%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8116171750

Skype: jjjimeneza

pradip kumar Sil

unread,
Jan 15, 2016, 11:29:07 PM1/15/16
to materials-welding
ASME Code does not refer for any third party inspection during qualify any WPS. Client Standard may ask you for the Third party witness.Lets example Saudi Aramco WPS Qualification needs Saudi Aramco approved third party inspector witness. Pls check first Client specification.

José Juan Jiménez Alejandro

unread,
Jan 16, 2016, 9:18:02 PM1/16/16
to material...@googlegroups.com
The partner is asking about the code AWS D1.1, the WPS that talking is not under specification ASME.