Hello Mr. Mustaq,
You will have to also mention the service temperature and other requirements..
Generally for SA333GR 6 consumable used is E7018-1, ER 70-S2 which can give Impact properties upto minus 45 deg C with PWHT and Non PWHT also.
Best Regards,
Mohit Aggarwal.
CSWIP 3.1
Sr. Engineer-Welding.
Dear experts
I have ltcs material A333GR6 how to select the consumables for this material please tell me as I am not really aware
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dc1e199c-d241-488f-876b-73353c77568d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Filler Metal ASME is ER80SD2. Material SA333 GR 6 to chlorine pipeline.
Dear experts
I have ltcs material A333GR6 how to select the consumables for this material please tell me as I am not really aware