Cladding Welding

36 views
Skip to first unread message

PK M

unread,
Mar 30, 2021, 4:38:48 AM3/30/21
to material...@googlegroups.com
Dear Experts,

Any one have WPS for Inconel 718 , 625 , & 825 on materials ?

any cladding welding related Method statements or procedure.

Please share.

Thanks in Advance

PKM.

José Juan Jiménez Alejandro

unread,
Mar 30, 2021, 11:14:22 PM3/30/21
to material...@googlegroups.com
I am sending you two examples, if I am not mistaken, the Inconel is a P43 under the ASME scheme, but take this into account: they are only examples !, which will undoubtedly serve as a guide for you to do your own procedures.
Greetings!.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_nctizvkLKSf5ppt5hQ5vgQhasCcD9_VzGB32yWkqP4%2Brg%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SUMMIT MÉXICO - TPI

https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/

Móvil +52 1 812 352 4606

Skype: jjjimeneza





P43-P43 GTAW-SMAW.pdf