Can anyone please confirm the Minimum distance between Socket weld joint as per ASME B31.3 where its specified.

 

Regards,

 

Faizal

 

 

 

 

 

Amit Vishwakarma

unread,
Apr 23, 2017, 6:49:41 AM4/23/17
to Materials & Welding, FAI...@saudichevron.com
Please find the snapshot of the code for your refrence. 

Regards
Amit Vishwakarma
B31.3.jpg

Faizal, Majeed [c]

unread,
Apr 23, 2017, 6:49:44 AM4/23/17
to Amit Vishwakarma, Materials & Welding

Dear Amit,

 

I mean , what is the minimum distance between the nearest two socket weld joints.

 

faizal

 

 

From: Amit Vishwakarma [mailto:amitsp...@gmail.com]
Sent: Sunday, April 23, 2017 10:23 AM
To: Materials & Welding
Cc: Faizal, Majeed [c]
Subject: Re: WELD DISTANCE AS PER ASME [**EXTERNAL**]

 

*** WARNING: This email originated outside of the CPChem network. Use caution opening attachments, clicking web links, or replying. ***
-

Rameez khan RK

unread,
Apr 27, 2017, 2:00:08 AM4/27/17
to Materials & Welding, amitsp...@gmail.com, FAI...@saudichevron.com

Faizal

Maintain 50 mm (or) 4 times the pipe wall thick

which ever is less. 
for two welding joint distance  

Regard

Rameez khan

pavan kumar reddy Juturu

unread,
Apr 30, 2017, 11:17:58 PM4/30/17
to material...@googlegroups.com

Dear Sir,

The distance between two weld joints should be 4 times the pipe wall thickness or one time the diameter of pipe but never closer than 1.5 inch. This is supposedly to prevent the overlap of HAZ of two joints.

Thanks and regards,
Pavankumar Reddy.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2609A8F1CC683C46AAF25170C11C6B6D0A5C2E7B%40cpamsaaj-msx05.am.cpchem.net.
For more options, visit https://groups.google.com/d/optout.

J Prinsen

unread,
May 1, 2017, 3:07:50 AM5/1/17
to material...@googlegroups.com
Is that code requirement or nice to have?
HAZ is normally no more than 2-3 mm
If it is code please give paragraph number
 
Kind regards


Van: "pavan kumar reddy Juturu" <pava...@gmail.com>
Aan: material...@googlegroups.com
Verzonden: Zondag 30 april 2017 15:58:31
Onderwerp: Re: [MW:26493] RE: WELD DISTANCE AS PER ASME [**EXTERNAL**]
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO4WkW%3DFVK2WJxt%2B9qkRkK8FJLaabdAhq__w9AfZ7DU9swBJPw%40mail.gmail.com.

hajarath ali

unread,
May 2, 2017, 2:46:40 AM5/2/17
to Materials & Welding, FAI...@saudichevron.com
Not required any minimum distance between Socket weld joint as per ASME B31.3.

Referance : 

B31.3 Interpretations No. 14 Interpretation: 

Question (4): Does ASME B31.3-1993 Edition, Addenda b, have requirements for the minimum lengths of pipe sections between welds? 
Reply (4): No
ANS.png
Reply all
Reply to author
Forward
0 new messages