6Mo weld to 6Mo | |||
Cr | Ni | Mo | |
A312 S31254 (6Mo) | 19.5-20.5 | 17.5-18.5 | 6-6.5 |
A312 S31254 (6Mo) | 19.5-20.5 | 17.5-18.5 | 6-6.5 |
ERNiCrMo-3 | 20-23 | 58 min | 8-10 |
Weld metal required | 19.5 | 17.5 | 6 |