Dear experts,
I need to procure this material
Hex Bolt & 2 nuts M20 x 75 based on ISO 3506-1 / A4-80 based on your experience, could you give me your feedback about material certificate, tests requirements and which I need to work with.
Thanks
ludmila
Hi
Required 3.1 certificate or coc as per client requiredment / mar / mr.
If 3.1 certificate is required, chemical and mechanical properties / values shall be indicated on the certificate along with pmi report.
Check also is there any external coating required as per client spec
Regards
Govindan
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1B0224B9A78AB34285E27B011195A046AA6F2F213E%40AOEPTTA-EG11.main.glb.corp.local.
For more options, visit https://groups.google.com/d/optout.