Hi,
We need to follow BS EN 9606-1 which supersedes BS EN 287-1.
In BS EN 9606-1, Clause 9.3 has been introduced regarding revalidation of a welder's qualification.
Regards,
Deepak Das.
Dinesh Gaur
unread,
Dec 31, 2015, 2:37:26 AM12/31/15
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Sign in to report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Dear Uday
This British Standard is the UK implementation of EN ISO 9606-1:2013. It is identical to ISO 9606-1:2012. It supersedes BS EN 287-1:2011 which is withdrawn.
moksh...@yahoo.co.in
unread,
Dec 31, 2015, 2:37:53 AM12/31/15
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Sign in to report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Sent from my ASUS
-------- Original Message -------- From:udaya bhaskar Sent:Wed, 30 Dec 2015 19:19:08 +0530 To:material...@googlegroups.com Subject:[MW:24017] DIFFERENCE BETWEEN EN-287 OR EN-9606.
--
A Comparison of BS EN 287 Part 1.2011 with BS EN ISO 9606: Part 1 - Job Knowledge 130.pdf