Good day all my dear experts,

Please clarify?

1). I have 3G P1 materials( thk 22 mm)WPS &PQR .
can I qualify for 2G,6G(dia 6")WQT on this WPS.

2).Possible to qualify 6G WQT on 5G fixed pipe WPS(Dia >24") thk 9mm

Karthik

unread,
Jan 18, 2020, 11:37:32 PM1/18/20
to material...@googlegroups.com
Hi, for WPS, position is not an essential variable. You can use WPS qualified with any position.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RMUjPMW0Ud8weSRgarP5NrpSAhO2i7_hxRO3AH8V89snw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages