Hi friend,
There is no restriction to SMAW. (subjected to a qualified WPS)
Better you show the setup requirement for SAW to the client and let him understand, hope he will get convinced,.
Thanks & Regards,
Lakshman Kumar B,
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No restriction in welding process, however we have to convenience client or try SAW it situ methods
Hi friend,
There is no restriction to SMAW. (subjected to a qualified WPS)
Better you show the setup requirement for SAW to the client and let him understand, hope he will get convinced,.
Thanks & Regards,
Lakshman Kumar B,
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Prasad
Sent: Saturday, February 27, 2016 12:27 PM
To: Materials & Welding
Subject: [MW:24384] Welding by SAW process is it mandatory for heavy thick vessels in H2 service
Dear welding experts,
We are manufacturing heavy wall vessels for H2 service.
MOC SA 516 Gr 70. Thick 56 mm
Due to large size vessels are to be supplied in two sections.
Hence on site weld joint will have to be done at place of installation.
At shop we are using SAW process for welding.
At field rotating is not possible and we want to use SMAW process.
Our client is asking us to use SAW process for field weld joint also.
We know that SAW is semi automatic & more productive process.
My question is whether is their any restriction to use SMAW process.
Request experts to give their valuable views to convience client technically.
Best regards,
Prasad Ghanekar
Thanks & Best Regards,
Pavankumar Reddy.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb19d5b1-6c54-45fe-8e91-1346dd8c9617%40googlegroups.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.
| From: Prasad Sent: Σάββατο, 27 Φεβρουαρίου 2016 - 09:02 To: Materials & Welding Reply To: material...@googlegroups.com |
Subject: [MW:24384] Welding by SAW process is it mandatory for heavy thick vessels in H2 service |
Dear,
You can use any welding procedures at site as per difficulties, subjected you shall provide an approved WPS/PQR for that thickness limit..
Regards,
Mohammed.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVidRd4PZxs%2B25s%2B_uKGftiGTeKfqoEidSica8Qo1_XNEA%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160227154234.6713426.85120.1966%40gmail.com.
Get your own FREE website, FREE domain & FREE mobile app with Company email. | Know More > |