UTS from hardness

84 views
Skip to first unread message

Priya Deshmukh

unread,
Aug 2, 2020, 6:29:51 AM8/2/20
to materials-welding
Hello All, 

I've measured hardness for my job using portable hardness tested in BHN. Can I calculate UTS of the job from the hardness values.

Thanks in advance, 

Priyanka Deshmukh. 

Harish Kannepalli

unread,
Aug 2, 2020, 6:32:44 AM8/2/20
to material...@googlegroups.com
Hi,
   You can use hardness conversion tables only for non austenitic steels.

Regards,
Harish Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFwED4XJ4op__Cu3yGm5r5P4%3D9jg2ggXSR1ZK6y9LwUeawrMkQ%40mail.gmail.com.

Rahul Rathod

unread,
Aug 2, 2020, 8:57:54 AM8/2/20
to material...@googlegroups.com
ASTM A 370 specification gives approximate hardness conversion numbers for some materials. See it. I hope it is useful for you, also you can use chart to convert BHN to tensile strength value, 

Please Check this link  https://www.ctemag.com/news/articles/tension-testing-or-calculation  Maybe it's helps you.

With Regards


 

Rahul J Rathod 

Senior Welding Technician 

What's up  +9181155889118

Email:  welder....@gmail.com


 view my profile onLinkedInview my profile on facebookmy skype id



sachit yadav

unread,
Aug 2, 2020, 11:01:43 AM8/2/20
to material...@googlegroups.com
You can Refer Astm A 370 _68..however it has limitations and  is not applicable for all materials..it shows approx.values.

Need to conduct Tensile test for reliable value of tensile strength. 

Rgrds

On Sun, 2 Aug 2020, 15:59 Priya Deshmukh, <piyuwi...@gmail.com> wrote:
--