Pressure Chart Recorder

0 views
Skip to first unread message

Mahmood Alhinai

unread,
2:39 AM (7 hours ago) 2:39 AM
to material...@googlegroups.com
Dear experts,

Kindly advise if any code or standard specify to use pressure chart recorder for piping spools hydrotest.

The client asking to use it although it is not mentioned in the approved procedure/ITP.

Please advise.

Thanks,
Mahmood

Tajuddin Mohammed

unread,
2:43 AM (7 hours ago) 2:43 AM
to material...@googlegroups.com
Pressure chart recorder is normallly used in buried pipelines morethan 10% of its length

Thanks & Regards
Mohammed Tajuddin
WELDING INSPECTOR CSWIP 3.1
Contact  0530833486
JUBAIL



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANV5n6ja_XKiu8F5BBpa0vK0hW-CeJ%2BgttfPDuecYvdJfmUz%2Bw%40mail.gmail.com.

venkateswara reddy Desireddy

unread,
4:18 AM (6 hours ago) 4:18 AM
to material...@googlegroups.com
If you have agreement with enduser then recorded mandatory.As per ASME codes recorder not mandatory.