Hydrotest Procedure - 22,500 psi

45 views
Skip to first unread message

williams p wilson

unread,
Nov 9, 2022, 2:40:23 AM11/9/22
to material...@googlegroups.com
Dear Experts,
Greetings!!

Kindly please share the hydro test procedure for high pressure pipe lines fabricated under API 6A.


Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

Mostafa DAIF

unread,
Nov 9, 2022, 3:12:40 AM11/9/22
to material...@googlegroups.com
Hi Mr. Williams,

I have attached the procedure for your reference.

Best Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7a2PE-MKuAMYBEVk3RgAWZuNU0fGWunvU_Ki_7gzRnAQ%40mail.gmail.com.


--


Mostafa DAIF  CHEF PREPARATEUR
T:  05 23 38 90 72   F:05 23 34 53 75   M:  06 61 54 12 95 ,  mostaf...@taqamorocco.ma
 
Jorf Lasfar Energy Company PB 99 Sidi Bouzid - El Jadida 24 000 - Maroc
http://www.taqamorocco.ma
 
TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies.
 
The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (“TAQA”) or one of its affiliates.
Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful.
If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments.
Construction porcedure for ¨Pressure test piping.pdf