  Dear Team,

We are quoting on piping project as per B31.3,

During the tender we noted the point as 

" All the Extend of NDE Shall be as per code requirement "

Can anyone tell us where the extent of NDE mentioned in the ASME B31.3.
As per my understanding all the NDE requirements shall be NDE class of piping.

Please advise if anyone knows of the above situation.

Chip Frizzell

unread,
Oct 3, 2022, 11:51:17 PM10/3/22
to material...@googlegroups.com
Chapter VI Inspections & Examinations explains the minimum requirements for examinations per service classification  The 2014 version in part says 341.4.1 Piping in Normal Fluid Service shall be examined to the extent specified herein or to any greater extent specified in the engineering design.
(a) Visual Examination. At least the following shall be examined in accordance with para. 344.2: (see 1-6)
(b) Other Examination
(1) Not less than 5% of circumferential butt and miter groove welds shall be examined fully by random radiography in accordance with para. 344.5 or by random ultrasonic examination in accordance with para. 344.6. The welds to be examined in each designated lot shall include the work product of each welder or welding operator whose welds are part of the lot. They shall also be selected to maximize coverage of intersections with longitudinal joints. When a circumferential weld with an intersecting longitudinal weld(s) is examined, at least the adjacent 38 mm (11⁄2 in.) of each inter- secting weld shall be examined. In-process examination in accordance with para. 344.7 may be substituted for all or part of the radiographic or ultrasonic examination on a weld-for-weld basis if specified in the engineering design or specifically authorized by the Inspector.
It goes on to define requirements for other service classifications and conditions. 

Thanks,

Chip Frizzell 

CWI / ASNT NDT LVL III / CRI / NACE CIP LVL 2-Certified


Price is what you pay-value is what you get. 
Seldom does the lowest price result in the best value!

Sent from my iPhone

On Oct 3, 2022, at 9:19 PM, Anand Elankumaran <email2...@gmail.com> wrote:


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChxzag8Q6KzfjPf7q%3DGDY4EVSW_KBeaez%3DHrpBaaF_CzAA%40mail.gmail.com.

pgos...@rogers.com

unread,
Oct 4, 2022, 12:01:37 AM10/4/22
to material...@googlegroups.com

Please refer this clause: 341.4 Extent of Required Examination and read between the lines for all classes of piping covered by B-31.3 code. This clause  elaborated is as follows:

  • 341.4.1 Examination Normal Fluid Service.
  • 341.4.2 Examination Category D Fluid Service
  • 341.4.3 Examination — Severe Cyclic Conditions.
  • 341.4.4 Examination Elevated Temperature Fluid Service

 

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

--

https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChxzag8Q6KzfjPf7q%3DGDY4EVSW_KBeaez%3DHrpBaaF_CzAA%40mail.gmail.com.


Virus-free.www.avg.com

Anand Elankumaran

unread,
Oct 4, 2022, 12:05:37 AM10/4/22
to material...@googlegroups.com
Dear Mr. Chip Frizzell,
Thanks for the swift reply on the below querry.

Now i understand fully about the requirement and Once again Many Thanks.

 Regards, 
E. Anand

pgos...@rogers.com

unread,
Oct 4, 2022, 8:45:25 AM10/4/22
to material...@googlegroups.com

 

Please refer this clause: 341.4 Extent of Required Examination and read between the lines for all classes of piping covered by B-31.3 code. This clause  elaborated is as follows:

  • 341.4.1 Examination — Normal Fluid Service.
  • 341.4.2 Examination — Category D Fluid Service
  • 341.4.3 Examination — Severe Cyclic Conditions.
  • 341.4.4 Examination — Elevated Temperature Fluid Service

 

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of Anand Elankumaran
Sent: October 3, 2022 2:43 PM
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:33526] Piping NDE Requirements

 

  Dear Team,

--

https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChxzag8Q6KzfjPf7q%3DGDY4EVSW_KBeaez%3DHrpBaaF_CzAA%40mail.gmail.com.


Virus-free.www.avg.com

Anand Elankumaran

unread,
Oct 5, 2022, 11:17:49 PM10/5/22
to material...@googlegroups.com
Reply all
Reply to author
Forward
0 new messages