WPS Requirements as per BS EN 15609 & 15614 |
||||||
Material |
Size |
Process(Est. Weld thk) |
Material Grouping as per PD CR ISO 15608 |
Suitable Consumable |
Remarks |
|
GTAW |
SMAW |
|||||
1.4571EN X 6 CrNiMoTi
17 122 to |
22.3 X 2.77 |
GTAW (2.77) |
8.1 |
ER 316L-17 |
-- |
(Exaton 316/316L-17) |
1.4571EN X 6 CrNiMoTi
17 122 to |
168.3 X 10.97 |
GTAW + SMAW (4 + 6.97) |
8.1 |
ER 316L-17 |
E 316L-17 |
(Exaton 316/316L-17) |
1.7335EN, 13CrMo4-5 to |
33.4 X 3.38 |
GTAW (3.38) |
8.1 - 5.1 |
ER NiCrMo-3 |
-- |
|
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChwvFgCTrAHGN4Jp62zbaUGPfo%3D2YjVi7Vn8y44q9eufcQ%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNFMDnEksFYoUNmh%2BM%2Ba4LkFJpkWjhxWELKMX3WZ5%2B0WQ%40mail.gmail.com.