There is no requirement as the standard uses "may" for the heat treatment which is normalization and shall be done before the test.
The requirement is about the pipes that will subject to heat treatment in their production process and they shall subject to same heat treatment after the flattening test.
Refer design code for pwht not 370.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/04685247-b286-427c-88f9-6dd67bc51daf%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.