Best Regards,
Krishana Kamal Nayan
QA/QC Engineer
Weatherford Oil Tool Middle East Ltd. |
Mobile:+964 780 925 0270
Krishan...@ME.Weatherford.com │ www.weatherford.com

Hello
It must be part of your own coating procedures and standards
If you don´t have it, you could approach to introduce it.
So, you must considerer type of soil, presence of contaminants and water, etc. to select the correct coat scheme
Regards
Miroslav Tadic
Ingeniero de Integridad
CEE
Gerencia de Producción - Mantenimiento
YPFB Chaco S.A.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAN%2Bgo9C52HC_pkLCfHbgHxntO9XPsqJW2g6wapeMxpVe6y50aQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Best Regards,
Krishana Kamal Nayan
QA/QC Engineer
Weatherford Oil Tool Middle East Ltd. |
Mobile:+964 780 925 0270
Krishan...@ME.Weatherford.com │ www.weatherford.com

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/B1C5C970BEA29243935FA5EB72F113C8026B740DA5%40BOLEXVSG11.chaco.com.bo.