Dear Experts,
As per b 31.3 Joints can be painted before leak test. Is the leak test referred here as a hydrotest also? Please confirm.

image.png

Best Regards,

 

Krishna Kamal Nayan  


 

Karthik

unread,
Oct 12, 2021, 7:59:43 AM10/12/21
to material...@googlegroups.com
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN%2Bgo9BBYPf%2BLOCJ-S-7BfZDce_oxVfV1gqYpr7WKeg5m5eb%3Dg%40mail.gmail.com.

Sagar SK

unread,
Nov 29, 2021, 10:14:22 PM11/29/21
to Materials & Welding

345.3 Preparation for Leak Test
345.3.1 Joints Exposed
(d) All joints may be primed and painted prior to leak
testing unless a sensitive leak test (para. 345.8) is
required.

Regards,

Peter Soloman

unread,
Dec 6, 2021, 11:34:24 PM12/6/21
to Materials & Welding
Dear All,
Yes...The leak test means  Hytrotest also.
Regards,
SOLOMAN PETER
TTSJV Project
Bahrain

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Vinay Thattey

unread,
Dec 8, 2021, 1:21:07 AM12/8/21
to material...@googlegroups.com, kkme...@gmail.com
Yes. Hydrotest is leak test..Other sensitive tests are bubble,sniffer...But in my view, hydrotest is leak test.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Mhaskar Aly

unread,
Dec 9, 2021, 10:39:58 PM12/9/21
to material...@googlegroups.com
Pressure Test and Leak test are two different tests; used for different purposes.

--