Experts,
We have received Female Sprinkler Head Adaptor 3/4”* 1/2” size.This adaptor shall be made socket weld with 1" Pipe. But ID for the 1” pipe is 25 mm and id for Female Sprinkler Head Adaptor 3/4”* 1/2” is 27.5 mm (Pls see the attached pics ).
If we weld Pipe to adaptor , we will not be able to get Weld penetration with this size deviation.
Can we do Butt Weld in this case?
Kindly advice.
Best Regards,
Krishana Kamal Nayan