Dear Experts,
We have one PQR and WPS parameters as below:
1. Code: AWS D1.1/D1.1M : 2015
2. Material & Grade: A36M.
3. Position: 1G, 2G.
4. Backing: back weld
5. Welding process: FCAW GS (Semi-auto).
AWS
D1.1, Table 4.5 & Table 4.6 did not state the essential variable /
requirement in same welding process if we use a weld technique by Semi
Auto method in the PQR then convert to Automatic method on
production or vice versa.
Please advise on this issue whether
still acceptable to change FCAW GS semi auto to FCAW GS Auto process or viceversa
Best Regards,
Chandra