Dear Experts,
We have a pump impeller with crack for repair. The material specification
for this impeller is Aluminum Bronze Casting (AlBC3 / ASTM C95800).
With this regards, what should be the appropriate welding filler or
electrode to be used for this type of material?
Thanks in advance for your support.
Best regards,