Dear experts,

One of our suppliers proposed to carry out Glass Bead Blasting on SS 347 ID surface.

Is there any ASTM specifications and standard and is this method acceptable?

Pl share your views.

Kannayeram Gnanapandithan

no leída,
3 mar 2020, 0:07:093/3/20
a materials-welding
Yes

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2rUpUd-3L4E-1g5XOwRDS2fOoC2mY%3DD2ZFeczbt77zaRw%40mail.gmail.com.

Hrushikesh Sangamnerkar

no leída,
3 mar 2020, 0:44:513/3/20
a Materials & Welding
Sir pl share the specification or reference standard