Dear experts,
I have a P8 # P43 PQR.
Joint design = Single V
Base metal thickness for P8 = 40mm and for P43 = 20mm.
What should be the Max.Base metal thickness range qualified for such joint?
Regards,
Hrushikesh H Sangamnerkar
The qualified thickness are as follows:
Thinner member: from 5 mm to 40 mm
Thicker member: no limitation
Please refer to QW-202.4 in Section IX of ASME BPVC
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Hrushikesh Sangamnerkar ---05/05/2015 15:21:53---Dear experts, I have a P8 # P43 PQR.
Regards,
Hrushikesh H Sangamnerkar
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2oHcKgDYmxWs9gVLaM8WLSSCewN4XcECCjVs6i8fkr7jw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
Are you qualifying PQR with taper on one side of higher thickness i.e. 40 mm.
Best Regards,
Mohit Aggarwal.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2oHcKgDYmxWs9gVLaM8WLSSCewN4XcECCjVs6i8fkr7jw%40mail.gmail.com.
No I already hv this PQR
Hrushikesh H Sangamnerkar
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPNyF3xTa-YFhKEqaC_1ixrNH%2BShPV-5m%2Bc2bH%3DcyFCERg%40mail.gmail.com.