Hi Gents,

Could you please advise ; does RWC (ISO 3834-2) can issue/sign WPS & WPQR and is it requirement of Standard/Codes that  RWC should has a IWE Diploma for this?.



Regards,
Ilkin HASANOV

Kannayeram Gnanapandithan

unread,
Mar 30, 2021, 11:14:02 PM3/30/21
to materials-welding
Not mandatory but u should have sufficient knowledge experience in welding. 3834 system for qualification fusion welding of shop. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ae3963c3-d53c-4bfa-a484-e59726641cc7n%40googlegroups.com.

nandagopal k

unread,
Mar 30, 2021, 11:14:02 PM3/30/21
to Materials & Welding
Dear ,

Pl Refer  the  web Link 


--

Dhatchana moorthy.S

unread,
Mar 30, 2021, 11:14:02 PM3/30/21
to material...@googlegroups.com
Please refer ISO 3834-5, Annex A. 
I think you can sign the document. 


--

Ramesh

unread,
Mar 31, 2021, 1:03:16 AM3/31/21
to material...@googlegroups.com
Where do you want to sign on WPS/PQR ? as a preparer or checker or approver ? 
You may not sign in any of these areas,  The role  is to perform quality checks during manufacturing  and it shall be defined by your QA/QC manager / Document systems. 
 
You can assist IWE/IWT for preparing WPS/PQR , but the final responsibilities lie with the IWE/IWT holder only. 
Even some case, IWT holders sign itself not accepted by some clients

Refer ISO 3834-2 , Clause 7.3
image.png

Also, as per above link, 

It's clear that RWC is not a portable title since There is no actual qualification for personnel responsible for welding coordination. 
only IWE, IWT , IWS  have been accepted as satisfying the specific knowledge requirements for Responsible Welding Coordinators.


Thanks and Regards

Rameshkannan D

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



--

Ramesh

unread,
Apr 1, 2021, 5:10:58 AM4/1/21
to material...@googlegroups.com
Further to my previous email,

I found the below page in IWE course material. 

image.png

Thanks and Regards

Rameshkannan D

Personal Mobile : 0091-9894987227

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"

Kannayeram Gnanapandithan

unread,
Apr 1, 2021, 7:10:03 AM4/1/21
to materials-welding
ref iso 14731

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Reply all
Reply to author
Forward
0 new messages