Dears
         Construction Code-ASME Sec 8, Div-1.   Nozzle hole is fouling in the  Welding of Dished End Petal Construction. Is it permissible?. Throw your valuable inputs. 
 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

Ramesh

unread,
Mar 7, 2020, 4:50:02 AM3/7/20
to material...@googlegroups.com
image.png
image.png
Generally client will restrict any openings in pressure retaining welds, however code requires additional RT 

Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePwMfsfsPEWEwe8beOO8NQVY-8EPrkxMc%3DF_jFFKnV6hA%40mail.gmail.com.

nandakumar pandit

unread,
Mar 7, 2020, 4:50:02 AM3/7/20
to material...@googlegroups.com
You have not mentioned joint effect. If the construction is with full radiography, you can go ahead.
N. S. Pandit

--

José Juan Jiménez Alejandro

unread,
Mar 7, 2020, 4:50:02 AM3/7/20
to material...@googlegroups.com
Please see: UW-14 OPENINGS IN OR ADJACENT TO WELDS.
Regards!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePwMfsfsPEWEwe8beOO8NQVY-8EPrkxMc%3DF_jFFKnV6hA%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro