Dear Vijay,
The above query is related to me also, can you please explain in detail.
And I have qualified PQR, please refer to I have included the two different PQR range.
Material Both PQR ASTM A106 Gr B
Thickness Range - 5 mm to 25 mm
First PQR Range -
| POST WELD HEAT TREATMENT( QW-407) |
|
|
|
| TEMPERATURE RANGE |
630 ±10° C |
|
| SOAKING PERIOD |
190Min |
|
| HEATING RATE |
190°C/Hours Max |
|
| COOLING RATE |
190°C/Hours Max |
|
Second PQR Range -
TEMPERATURE RANGE TP1 - 638 ±10° C TP2 - 635
±10° C
SOAKING PERIOD: TP1 - 72 min TP2 - 189 min
HEATING RATE: TP1 -170°C/Hours and TP2-171°C
COOLING RATE: TP1- 163°C/Hours and TP2-106°C/h
But it is not clear to me how to confirm if mechanical properties are ok after just one PWHT ( for sure Tensile St. and Y. S. will be ok, since values are greater, but hardness test?
Please explain to me about the mechanical test and 3 cycles PWHT. Where I require test coupons for first PQR.
Thanks and Regards
Kiran