NDE REQUIREMENT FOR P11 MATERIALS AFTER PWHT

110 views
Skip to first unread message

V.kishore raju

unread,
Aug 25, 2022, 4:32:28 AM8/25/22
to Materials & Welding
Dear all
can i perform NDE inspection like RT,HT,MT,PMI before 48hrs from the pwht time for P11 materials,is there is any specific code regarding this matter.
kindly conform me.

thank you.

Ajay Gupta

unread,
Aug 25, 2022, 5:13:15 AM8/25/22
to material...@googlegroups.com
That will not be any problem, please ensure NDT shall be carried out after 48 Hrs of PWHT not immediately after heat treatment.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cf61cc50-a0d5-4151-b940-15a1122c12cen%40googlegroups.com.

Kannayeram Gnanapandithan

unread,
Aug 25, 2022, 5:50:42 AM8/25/22
to materials-welding
REF ASME B31.1,  136.4, No time limit but for materials like P3,4,5 etc, NDE is to be done after PWHT only unless otherwise specified

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Aug 25, 2022 at 2:02 PM V.kishore raju <vkishor...@gmail.com> wrote:
--

Ganesh Rao

unread,
Aug 25, 2022, 5:50:48 AM8/25/22
to material...@googlegroups.com
As my experience after 24hrs once done PWHT can be processed to all kind of NDT