Dear Vikas,
Yes.
If the Client specifications say so than you need to follow it or else provide technical justification based on NACE standards to over rule the client spec.
Generally the order for precedence are you local regulations, contract documents than project specifications and lastly the international Codes and Standards.
Regards,
PARAG PANSARE
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f9e7e0e1-561e-4e7e-9a72-214aa7468fe3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Dear Sir,
You have to follow client specifications. It is the designer who decides whether pwht is needed or not in these cases.
Regards,
Hareesh K V
+91-8547859202
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4e09e9f0-7c70-4749-afbd-dcf9bd3b2255%40googlegroups.com.