Gent's
Can any one explain with example of thickness qualifications - procedure.
Especially for combination of process with 19mm to 38mm thickness job welded.
Explain me each and every step.
Here I explain what I am understand that code. Weather it's wrong please explain.
Example.
Job PQR thickness - 25.4mm
Process - GTAW (4mm)+ SMAW(21.4)
as per ASME sec IX, Qualifications range for GTAW 4mm --- min - 5mm, max- that is <19mm, 2t =8mm
Qualifications range for SMAW 21.4mm -- min-5mm, max- that is >19mm, 2T=2(25.4)=50.8mm
So..
The total thickness welded is 25.4(4+21.4)mm
Total thickness qualified is -=8+50.8=58.8mm
Is that correct or not.
If it wrong kindly give me a brief lesson to me.
Thank you
Ganesh
QC Welding