Hi allWe have a pqr qualified without backing and back weld, we have prepared a WPS without back weld, can I use the single WPS for joints with back weld
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALwNT%2B_AoaeESuhU3J3O%3DVJS%3DK5X_t268_TsLOoKS4dRFusqxA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.