Dear experts,
We need your kind support based on your experience and any code/std references.
The situation is that some of our process piping in refinery division THE CIRCUMFERENTIAL JOINT has come such position that the joint rests on the structural beam.
Is it allowed?
Some inspector have a concern that there is a developed stress while operation and the joint may fail.
Please share your experience and reference.
Thank you very much
With best regards
Biplab Pal
--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:
bipla...@gmail.com Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAFnzQg22xWSiTOEonpZtZCDqBZ9vvh9OGZ_bKvHJ9CrS1L-qSg%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.