to material...@googlegroups.com

Dear Expert,
Can we use ER316 for welding of SA312 TP316H piping by GTAW process.
Regards,
Sachin

Vanchinath S.A.

unread,
Jan 15, 2016, 11:19:19 PM1/15/16
to material...@googlegroups.com
make sure ER 316 wire used has min carbon of 0.04%

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuWLDLn7AmSMisAkc4eL8kDDt4jQQ01YR66MPOsziVZ5FfZAw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Mohd Siraj

unread,
Feb 4, 2016, 4:59:01 AM2/4/16
to Materials & Welding
Can we use ERNiCrMo3 ??