IS IT POSSIBLE TO MAKE SPLIT TEE BY CUTTING ORDINARY TEE

74 views
Skip to first unread message

afzal ahmed

unread,
Feb 9, 2015, 3:14:41 AM2/9/15
to material...@googlegroups.com, Afzal Ahmed
Dear Friends please Help me ,
 
We need Split Tee of 6"(SMLS SCH 40 ASTM A234 GR WPB) , but it is not available in market easily ,
1: Is it possible to make Split Tee by cutting ordinary Tee vertically
2: if Yes, then in which STD it is telling
3: & what are the NDT requirements
 
for more clarification See the attached file
 
its very urgent .....
 
 
20150209080928378.pdf

Umar Rashid Makrani

unread,
Feb 9, 2015, 4:12:37 AM2/9/15
to material...@googlegroups.com
If you have a tea of ASTM A234 and you cut it into 2 halves. The material is still ASTM A234 so I believe this can be used.

 
With Best Regards,
Umar Rashid Makrani, PMP® ,


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0656b478-8126-4723-92b4-e58408747f3b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

abdulrauf1947

unread,
Feb 9, 2015, 5:22:24 AM2/9/15
to Umar Rashid Makrani, material...@googlegroups.com
Either get approval from client or get its approval from design and proceed .

.... No issue
Regards; ar
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJCSKyhA%3DTJ1cFUghZ06pVB5c%2BNb0mVba2FuFcm3k8D3hh9TcA%40mail.gmail.com.

afzal ahmed

unread,
Feb 9, 2015, 9:53:44 AM2/9/15
to material...@googlegroups.com, afzalm...@gmail.com
WHAT ABOUT  THE NDT REQUIREMENTS?

afzal ahmed

unread,
Feb 9, 2015, 12:12:08 PM2/9/15
to material...@googlegroups.com, firoz....@gmail.com
But on what basis client will approve it?
which STD?

Umar Rashid Makrani

unread,
Feb 11, 2015, 3:34:17 AM2/11/15
to material...@googlegroups.com
My apologies for a wrong spelling,
I my idea was that if a material is manufactured A234 it will remain A234 even after you cut it, I don't think we need to look for a code citation. Regarding the NDT if its cut by machining no NDT is required again however as per the need the edge of the new half tee can be tested by PT to ensure that its defect free and suitable to weld.

 
With Best Regards,
Umar Rashid Makrani, PMP®

afzal ahmed

unread,
Feb 11, 2015, 6:13:56 AM2/11/15
to material...@googlegroups.com
what about after welding ? which NDT method we need to follow ?

Mohan q8

unread,
Feb 11, 2015, 9:27:34 AM2/11/15
to material...@googlegroups.com
Dear Afzal,
 
Need further details about the pupose of spilt tee.
 
In gneral if you want to use the splilt tee for hottap/tie-in purpose you need to split in horizondal portion of the tee.
Moreover, if your want to use the spilt tee over the pipe you cann't able fit it properly due to ID of the tee will not match with OD of the pipe and also you will find gap between halfs after fit-up.
 
Welding & NDT:
 
In case of welding Spilt tee over the pipe, it will be welded with backing strips.
 
Root/first pass - DPI
Final - MPI
Test - Hydrotest of stub.
 
 

 
On Mon, Feb 9, 2015 at 11:14 AM, afzal ahmed <afzala...@gmail.com> wrote:

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0656b478-8126-4723-92b4-e58408747f3b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
With Regards,

Mohan, Q8.

afzal ahmed

unread,
Feb 12, 2015, 12:31:53 AM2/12/15
to material...@googlegroups.com
Actually we had constructed  storage tank of  MOLTEN NAPHTHALENE . so we need to Tie in with existing napthalene pipe line and for jacketing of SS pipe line coming from napthalene tank .

afzal ahmed

unread,
Feb 12, 2015, 12:35:23 AM2/12/15
to material...@googlegroups.com
We recieved Split tee. but the ID of split Tee is the OD of existing pipe . same thing u told before .....


On Wednesday, February 11, 2015 at 5:27:34 PM UTC+3, redbull wrote: