Subject:- Charpy Impact Testing on weld metal

51 views
Skip to first unread message

Shahil Saini

unread,
Dec 15, 2020, 11:58:49 PM12/15/20
to material...@googlegroups.com
Hello everyone, 

My question is, Why ASME BPVC and other standard codes discarded the 'U' notch impact testing?

George Dilintas

unread,
Dec 16, 2020, 10:47:12 PM12/16/20
to material...@googlegroups.com
V notch simulation is more reliable 

Στις Τετ, 16 Δεκ 2020, 06:58 ο χρήστης Shahil Saini <sainis...@gmail.com> έγραψε:
Hello everyone, 

My question is, Why ASME BPVC and other standard codes discarded the 'U' notch impact testing?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_9KBo5H3LU6KOD1xU1LpWHVZwm5SJq4-Z%3DkQDprJTQTrw%40mail.gmail.com.

Shahil Saini

unread,
Dec 17, 2020, 11:37:37 PM12/17/20
to material...@googlegroups.com
That I know sir, but I want some more information behind this topic why they discarded U notch and For every material they are not using U notch or for which materials U notch is used?

pgos...@rogers.com

unread,
Dec 18, 2020, 12:07:16 AM12/18/20
to material...@googlegroups.com

U- Notch for Charpy impact tests used to be followed  DIN standards, back in 1970s. In fact DIN standards used to provide an option for both Notch types. Correlation of impact data was never easy.   It’s discarded since then.

It’s a matter of basic understanding : a V notch generates more stress than an U-Notch, Hence materials exhibiting good impact with V Notched specimens  would easily meet the criteria in U-Notch conditions not the other way. Notch toughness is an extremely critical property for engineering design.

Anything good under worse condition(V-Notch) is more reliable that something performed under ideal condition (U-Notch). Engineering codes, material properties  have matured  and improved leaps and bounds over the. Hence adoption of V-Notch Charpy impact test is an example of that principle.

Hope it clears your doubts.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Saudi Aramco Approved Designated Welding Engineer(DPWR)

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

Shahil Saini

unread,
Dec 18, 2020, 7:46:21 AM12/18/20
to material...@googlegroups.com
Hello Pradip sir,
Sir, can you say about, any metallurgical difference we get on the fracture surface and is there any change in fractography on both v and u notch test samples  